Could someone explain me what is the Gurley method to determine the airflow through a material & give the relationship w/ the airflow in ml/(min.mm².mbar) ?
thx
 
Replies continue below

Recommended for you

Don't know if this helps...

Gurley numbers are used to indicate the relative permeability of membranes or materials...The number (in sec) is obtained by measuring how long a known volume of air at constant pressure takes to pass through a material.
Your constants would be air Pressure, Area of membrane...

Here is a website you might find interesting...
In the past, I've run across some good literature on this from WL Gore...the manufacturer of GoreTex!!
 