Jul 14, 2009 #1 99491 Mechanical Joined Apr 3, 2008 Messages 34 Location KE We have just begun a piping job where the client has stipulated that all pipes 2" and below are to be TIG welded regardless of what the pipe is carrying. Can somebody tell me why this may be?
We have just begun a piping job where the client has stipulated that all pipes 2" and below are to be TIG welded regardless of what the pipe is carrying. Can somebody tell me why this may be?
Jul 14, 2009 #2 Mr168 Materials Joined Aug 5, 2008 Messages 731 Location US Lower weld reject rates and fewer flow losses from protruding weld metal as opposed to stick root and fill is a good place to start. Upvote 0 Downvote
Lower weld reject rates and fewer flow losses from protruding weld metal as opposed to stick root and fill is a good place to start.
Jul 14, 2009 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Why don't you ask the client? Upvote 0 Downvote