GTAW WPS filler Wire size 2

Status
Not open for further replies.

Pipoy04

Mechanical
Joined
Nov 22, 2014
Messages
40
Location
QA
Dear All,

With regard to GTAW WPS, if the WPS mentioned that the filler wire diameter is 2.4mm but the available filler wire size for GTAW is only 3.2mm. Does we require to provide new GTAW WPS?
 
Hi,

What is the reference code for WPS qualification? If the qualification of welding procedure is based on ASME Section IX, you do not need to qualify a new WPS if the diameter of filler wire changes because it is a non-essential variable.
 
Dear Genetix,

We are working under ASME Section IX.

Thank you for the prompt response.

Is your reference Table QW-256 (GTAW)?
 
I agree with Genetix that a requalification is not required. However, a new or revised WPS should be written based on the same PQR referencing the 3.2 mm filler wire.
 
The welder is bound by the WPS. If someone listed a single diameter, then that is what the welder must use until someone takes the time to revise the WPS. There are occasions where there is a reason to list only one filler metal diameter, other times listing one diameter is because the person writing the WPS didn't know any better.

The same holds true for the weld type (fillet versus groove weld) as well as joint type (Tee, Butt, Corner, etc.), and groove type (V, J, square, etc.), groove angles, single pass versus multiple. the list includes any nonessential variable. If the WPS only lists one weld type, one groove type, etc., that is what the welder is limited to.

Best regards - Al
 
Simply revise the WPS to permit both (or more) filler metal diameters to be used.
 