What welding consumable can be used to weld (GTAW)Monel K500 to SAF2507 Super duplex, and what are the associated problems.
 
Tungsten electrode can weld (GTAW)Monel K500 with high quality, no contamination and excellent appearance.You can get them from us including pure tungsten,ceriated tungsten,thoriated tungsten electrode etc. with high quality and lower price.
 