Typical grout manufacture requires use of pea gravel for application deeper than 3". Is it really required or recommended? why?
 
Replies continue below

Recommended for you

Strictly speaking, you could use a sand/cement/water mix. But the gravel acts as a filler, and helps to reduce shrinkage.