I was recently reviewing a ground grid study for an indoor installation and saw something that struck me as odd. The ground grid is installed beneath the basement, air cured, concrete floor of a building. There is steel re-bar inside the concrete slab. Yet the study still lists the resistance of the slab as 10,000 ohm-meters. This seems high to me.

Has anyone had previous experience with this type of installation that could verify whether this is or isn't a plausible resistance value for air cured concrete with re-bar?

References to technical documents would be much appreciated. I have already looked through the office copies of IEEE 80, IEEE 81, IEEE 665 and the IEEE Green Book. I so far haven't been able to locate anything indicating the resistance of air cured concrete for indoor installations.
 
Replies continue below

Recommended for you

Concrete mixes using Type III Portland cement with ternary combinations of Class F fly ash, silica fume and slag could present up to 1000 ohm-m resistivity. See:
Usually under the concrete floor, it is an isolation layer –polyethylene or rubber
of 2-5 mm thick and this layer of high resistivity could influence the resistance measurement.
 
TSun,
Just for my own curiosity, why there is a copper ground grid under the steel re-bar concrete basement at the first place?
What type of electrical installation do you have?
 
It is a commercial building with indoor 15kV equipment. With the way they modeled the room, the ground grid is necessary to keep step and touch potentials to an acceptable level but I am not sure that the room was modeled correctly.
 