Hi All. I am investigating damage done to some steel brackets which connect a shipping container to four screw jacks used to level it. I have never been involved with the investigation of damaged steelwork before.

I want to confirm that there are no cracks at the welds using dye penetrant. However, the brackets are painted. I assume the paint will have to be removed by grinding to expose the welds below.

Is it possible that the grinding process might hide the cracks covering it with a thin layer of steel? (Similar to a burr on a knife. I am thinking malleability)
Is it possible that the grinding process might hide the cracks by filling it with paint swarf?

Thanks in advance
 
Replies continue below

Recommended for you

You may consider magnaflux as it can detect shallow cracks below the surface.

Your structure is likely a fairly ductile. I wouldn't expect cracking without significant deformation.
 
Gentle sandblasting will remove the paint without distorting the underlying metal. And a small air gun is cheap.
 