Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Green slime out of 115 volt receptical 11

Status
Not open for further replies.

frankiee

Marine/Ocean
Joined
Jun 28, 2005
Messages
138
Location
CA
No I do not smoke crack cocaine and I never have.
The situation is this:

Outdoor hut with an electric heater in it.

Used for an hour a day

The wire feeding the hut was a 16 gauge outdoor cord (no I did not put it on.)

Green liquid comes out of the slots
 
Just to clarify if it is corrosion product of copper. Take a small sample of the slime, putting it into a jar. To the jar add a 20 to 30 ml of household ammonia. Cap the jar and shake. If the liquid turn a royal blue then copper ions are present.

Vita sine litteris mors est.
 
Yep, that's the stuff alright. Strange thing is it never appeared until I stored the two items in my basement. Would radon gas (5-6 ppm measured) or hydrocarbons from my oil-fired boiler cause a chemical reaction with the PVC? That big puff of smoke whenever the burner kicks on probably isn't a good thing...
 
The green corrosion sometimes seen on copper is called Verdigris.

Here is a link ->

Also interesting to note; this is why it was very important to keep copper cookware tinned in a Victorian kitchen. It's poisonous.
 