Michael2009
Petroleum
- Jun 24, 2010
- 49
Hi,
I try to measure a GRE pipe with my multi meter. I am expected to get some mega ohm reading. But i getting totally open connection. (insulated)
that is require for GRE pipe to be conductive in hazardous zone. Vendor also claim their pipe is conductive type. But dont get the physical ohm reading. I am measure outside surface point to point in the same GRE pipe spool. I change to measure inside surface point to point. Is also same no conductivity reading.
I am not sure that should be other method of measurement not direct pulling multi meter on it or .. the GRE is non conductivity type.
Can you guys suggest me a method of testing the GRE pipe conductivity?
THanks in advance.
I try to measure a GRE pipe with my multi meter. I am expected to get some mega ohm reading. But i getting totally open connection. (insulated)
that is require for GRE pipe to be conductive in hazardous zone. Vendor also claim their pipe is conductive type. But dont get the physical ohm reading. I am measure outside surface point to point in the same GRE pipe spool. I change to measure inside surface point to point. Is also same no conductivity reading.
I am not sure that should be other method of measurement not direct pulling multi meter on it or .. the GRE is non conductivity type.
Can you guys suggest me a method of testing the GRE pipe conductivity?
THanks in advance.