MohdYaseen2010
Mechanical
Our case as follow;
GRE (API 15LR) pipeline with 41 Km length & difference of elevation (141 m @ source, 13m @ 32KM from source, 22m @ 41KM).
Pipeline Design Pressure (DP) is 2MPa for the first 32KM & 3MPa for the rest 9KM.
The Contractor has execute hydrostatic pressure in sections (4 sections) & now they want to join these section WITHOUT CARRY-OUT AN INTEGERAL HYDROSTATIC PRESSURE as they will make some lamination (or banding) on the intended joints.
Contractor excusing with that no regulation/standard/code enforcing doing the test for the whole pipeline as one section.
Our main concern is for the lowest point (@ 32KM from source) as it will be subjected to the highest pressure (it has lower DP compered to the subsequent part).
Please give me your idea, and share any reference if you have?
Mohd Yaseen
GRE (API 15LR) pipeline with 41 Km length & difference of elevation (141 m @ source, 13m @ 32KM from source, 22m @ 41KM).
Pipeline Design Pressure (DP) is 2MPa for the first 32KM & 3MPa for the rest 9KM.
The Contractor has execute hydrostatic pressure in sections (4 sections) & now they want to join these section WITHOUT CARRY-OUT AN INTEGERAL HYDROSTATIC PRESSURE as they will make some lamination (or banding) on the intended joints.
Contractor excusing with that no regulation/standard/code enforcing doing the test for the whole pipeline as one section.
Our main concern is for the lowest point (@ 32KM from source) as it will be subjected to the highest pressure (it has lower DP compered to the subsequent part).
Please give me your idea, and share any reference if you have?
Mohd Yaseen