Sep 4, 2014 #1 KMur Mechanical Joined Apr 27, 2007 Messages 40 Location AE Dear ALL, Where can I get the GRE limitaions in terms of pressure and temperaure? Please advise sutiable standards. Thanks
Dear ALL, Where can I get the GRE limitaions in terms of pressure and temperaure? Please advise sutiable standards. Thanks
Sep 4, 2014 #2 nickypaliwal Materials Joined Aug 28, 2014 Messages 199 Location OM SHELL DEP 31.40.10.19 for GRE Piping Upvote 0 Downvote
Sep 5, 2014 #3 SJones Petroleum Joined Apr 22, 2001 Messages 3,945 Location GB The pressure and temperature limitations come from the manufacturer supported by the required qualification test documentation that may be as per API Spec 15HR, ASME X, or ISO 14692-2 amongst others. Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
The pressure and temperature limitations come from the manufacturer supported by the required qualification test documentation that may be as per API Spec 15HR, ASME X, or ISO 14692-2 amongst others. Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer.