I'm am facing a situation where pipes delivered from pipe mill, normally ready to be coated, are in fact highly contaminated by graphite scale which we can not easily remove by standard water washing.

Do you have any suggestion?

Thanks

Lupo

 
Dear All,

thanks for the tips!
I have another question...which could be for you the effect any residual graphite onto pipe surface when heated at 240°C before application of the FBE?