Respected members,

I would like to know some technical details on granite/ stone look finish.

One reference here:
Link

This company don't supply outside USA. So to procure locally and to explain vendors I would like to know some technical specifications.

Kindly help me.

Regards,
 
It is a commercial/homeowner use void/crack sealer for hard surface materials . You can google the web to find hundreds of similar products.
 
The Daich Coatings website showing products out of stock.

There are couple of local vendors I found.

But I don't know how and what to verify in the product spec. Otherwise have to physically spread the coat and test those sample spreads. Any inputs please ...
 
specify and verify the following:

coating thickness
coverage
cure time
temperature limits
chemical resistance
application with trowel or brush or roller
surface sealant
epoxy - resin binder properties
warranty
aggregate gradation
primer / surface preparation required
 