Dear all,
Is there a way to use SAE Grade 8 bolts for ASME code applications? It seems SA354 Grade BD has comparable strength, but how do I re certify grade 8 bolts as SA354 Gr BD?
Thanks in advance for your help!
 
ME231;
The SA 354 specification for ASME Code application permits the use of any alloy steel as long as the requirements in Table 1, Hardness in Table 2 and Tensile requirements in Table 3 are met.

Certification per the above is described in Section 14 of SA 354. You will need to engage a reputable lab to perform the mechanical testing.
 

Thank you metengr for your quick comment. Is it too much wishful thinking, in your opinion, that bolt manufacturers could perhaps themselves sell us Grade 8 bolting certified as SA-354 or does tha vessel manufacturer usually have to do it himself?
 
Is the ASME Code in question a PV code or a piping code?

rmw
 
PV code - VIII-1 in particular
 
Is this a bolt for for a flange for an external connection, or a bolt for a flange integral to the vessel?

rmw
 
rmw, this is for an external connetion.
 
I think your answer is in this thread.

thread292-255131

However, if it is piping that is attached to your vessel and the piping is under the jurisdiction of any code, that code might dictate what your bolting options are.

rmw
 
thank you, rmw, for pointing me towards the right direction. I guess sticking to the code always does help. the thread was quite enlightening.
 