Hello,
which is the usual heat treatment for the grade 3?
i'm doing some tests with the samples normalized and tempering, but the impact test values at -101ºC, are quite low (about 5 to 12 j)
Any idea to increase this values? Maybe adding more Nickel to the steel? the Ni on the heat is quite close to the minimum requested by the norm.
thank you