Does anyone know a good reference for brazing A286 to 304L or 17-4PH to 304L? I am debating between BAg-3 or BNi. If the brazing temperature resolutions the A286, then I'll probably need BNi. Any advice? The alternative is to E-beam weld, preferrably JBK-75 instead of A286.