Iam looking for help/pointers for creating a gold solution for gold plating using 'pulse' technology. I have the guns made for 30AMP guns to do the gold plating. Any help is appreciated.
Thanks
 
Generally gold cyanide with e.g. potassium phosphate and/or citrate buffer.

Search for pulse plating, gold at e.g. <