Aug 9, 2004 #1 dpatlolla Chemical Joined Aug 6, 2004 Messages 2 Location US Hi Iam looking for help/pointers for creating a gold solution for gold plating using 'pulse' technology. I have the guns made for 30AMP guns to do the gold plating. Any help is appreciated. Thanks
Hi Iam looking for help/pointers for creating a gold solution for gold plating using 'pulse' technology. I have the guns made for 30AMP guns to do the gold plating. Any help is appreciated. Thanks
Aug 10, 2004 #2 nbucska Electrical Joined Jun 1, 2000 Messages 2,191 Location US Generally gold cyanide with e.g. potassium phosphate and/or citrate buffer. Search for pulse plating, gold at e.g. <http://www.google.com> <nbucska@pcperipherals DOT com> subj: eng-tips Upvote 0 Downvote
Generally gold cyanide with e.g. potassium phosphate and/or citrate buffer. Search for pulse plating, gold at e.g. <http://www.google.com> <nbucska@pcperipherals DOT com> subj: eng-tips