I know that gold will cause lead-tin solder joints to become brittle
over time, NASA tells me so. They have specific procedures to
avoid it. Has anyone seen anything in writing that goes into any
detail as to what the mechanism is and when to worry about
it? Thanks. Rick Schmidt
ricksintuc@yahoo.com

Mining, Mechanical and Electronics engineer.
 
Replies continue below

Recommended for you

Thanks for the tip. Unfortunately, there is a problem with the URL and I couldn't access the page?

Rick Rick Schmidt
ricksintuc@yahoo.com

Mining, Mechanical and Electronics engineer.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor