QW-404.32 For the low voltage short‐circuiting type
of gas metal‐arc process when the deposited weld metal
thickness is less than 1/2 in. (13 mm), an increase in deposited
weld metal thickness beyond 1.1 times that of the
qualification test deposited weld metal thickness. For
weld metal thicknesses of 1/2 in. (13 mm) and greater,
use Table QW-451.1, Table QW-451.2, or Tables
QW-452.1(a) and QW-452.1(b), as applicable.