Ok guys by no means am i the best welder out there
but i seem to have a hard time with Vertical up, solid wire. i am using argon gas C25
I can do it no problem with stick, or flux core wire ...
but solid is giving me a heck of a time
Settings are 170 amps
wire feed 145
i figure this should be low enough but still the bead is convex , can't keep it flat
anyone have suggestions?
thanks greatly appreciated
but i seem to have a hard time with Vertical up, solid wire. i am using argon gas C25
I can do it no problem with stick, or flux core wire ...
but solid is giving me a heck of a time
Settings are 170 amps
wire feed 145
i figure this should be low enough but still the bead is convex , can't keep it flat
anyone have suggestions?
thanks greatly appreciated