OK gentlemen and welders :) I am being told that under ASME sec IX if a welder Certifies under GMAW he is automatically qualified for FCAW using the same WPS I can't find anything under section IX that leads me to believe this. If you have an answer could you please reference code and sec.
 
Replies continue below

Recommended for you

Interpretation Number: IX-86-46
Codebook: Section IX
Volume: 20
Date: 24-NOV-86
Subject: Section IX, QW-355
Question: Is a welder who is qualified using gas metal-arc welding (GMAW) also qualified for flux-cored arc welding (FCAW) or vice versa, provided the other variables for performance qualification remain unchanged?

Reply: Yes.
 
According to AWS D1.1, the welding process is an "Essential Variable". Therefore welder re-qualification is required.

ref. D1.1 p152
 
Connectegr,
You would be correct if the question was about AWS D1.1.
 