Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Gluing PVC pipe to Rubber

Status
Not open for further replies.

friogatto

Marine/Ocean
Apr 6, 2005
9
I am trying to find a solvent and a type of soft rubber that I can use to glue the rubber to PVC.
it would go pipe to rubber tube back to pipe.
This will allow the pipe to bend gently (at the rubber area)and eliminate vibrations from a pump.
It would be under 10 PSI

any ideas would be greatful
 
Replies continue below

Recommended for you

Any polyester that uses styrene as a participating solvent.
Vinyl esters and their equivalents are suitable if water is present in service.
 
I would use Plyabond which is a neoprene rubber based solvent adhesive that will attack but not destroy the ABS
 
What are normal operating (or rated) temperatures for pvc sch#40 pipe?
How cold or hot until its properties change dramatically that it will lose its structural integrity?
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor