Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Geotextiles measurement

Status
Not open for further replies.

jamiejones16

Geotechnical
Joined
Oct 1, 2014
Messages
7
Location
AU
Hello! I researched about geotextiles but they vary in sizes. Now, I'd like to know the average measurements of every roll of erosion control geotextile.
 
I researched them as well but ended up reading information on how to measure geotextiles. But this may be come in handy for you.

NOTE: Measurements depend on the type of the fabric

COIR MATTING

Roll size 2 x 25m
Area covered 50m2
Thickness Light: 4.27mm Medium: 7.97mm Heavy: 9.12mm
Flow velocity Light: 2.5m/sec Medium: 3m/sec Heavy: 4.7m/sec
Tensile strength Light: 1208 x 690kg/m Medium: 1608 x 746kg/m Heavy: 2450 x 990kg/m
Weight Light: 400gsm Medium: 620gsm Heavy: 900gsm
Density material Light: 62% Medium: 57% Heavy: 41%

JUTE MATTING

Fine Weight 2m x 50m(280gsm)
Medium Weight 1.83m x 25m(750-800gsm)Slitted or non-slitted
Heavy Weight 1.83m x 25m(1300gsm)
Mats 370mm x 370mm (750-800gsm)
Mats 600mm x 600mm (750-800gsm)

You can view what it will look like when installed on a land site: Case Study on Geotextiles
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top