Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

GEC EM85 Gas Turbine Manual

Status
Not open for further replies.

Kiani1982

Industrial
Joined
Aug 23, 2015
Messages
3
Location
IR
Hello All,

I need some information or manual about GEC EM85, kindly contact me for that.

Regards
Kiani
 
Hello Hoxton,

Thank you so much for your swift response.

Unfortunately Greenray will not support this info to me, just I want to know how much is Turbine Inlet Temp (TIT) for EM85 and which material historically/technically used for Combustion Turbine stators Vanes 1/2 in the EM85.

We deal with a Non OEM, MFG for CT stator vanes 1&2 that the MFG made these vanes with Nimonic80A material, but the end user said Nimonic80 not suitable for this engine CT vanes 1/2 and should be use Inconel 738, Finally I want to know what I can do and who are right, becuase the MFG saying Nimonic80A is fine for CT Vanes 1/2.

Just we know Turbine Vanes Thermocouple show us 780 C during normal operation of GT.
Please send me your email address and cell No.


Regards,
Kiani
 