Exchanger tubesheet is duplex 2205. Channel is carbon steel. The tube fluid is cooling water (1500ppm Chloride, <50DegC). What is the gasket materials for channel flange, Carbon steel, 316L SS, or Duplex Stainless Steel?

Thanks.
 
Replies continue below

Recommended for you

silicone caulk? :)