hi all,

Can any tell me the properties of gasket material(soft steel or iron) at 65 deg.

I need modulus of elasticity, poisons ratio, density, thermal conductivity and expansion

thanks
 
Replies continue below

Recommended for you

what type of steel?

Patricia Lougheed

******

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.
 
I think the simplest answer is to go to Flexitallic's website or give them a call.

 
The material normally used in gaskets is referred to as ARMCO Iron.
Depending on your end use of the material you could get by with using the values for AISI 1010 steel.

Are you considering this for a gasket and if so, the need values for calculation of gasket seating stresses are in the code books or the gasket manufacturers catalogue.
 