Mar 19, 2007 #1 pipeJ123 Petroleum Joined Mar 19, 2007 Messages 2 Location NO Hi, Can anyone tell me if do I need to replace the existing gaskets installed between the spectacle blind and flange when I rotated the spectacle blind? The line will be pressure tested thus, I need to rotate the spectacle to close the line. Thanks
Hi, Can anyone tell me if do I need to replace the existing gaskets installed between the spectacle blind and flange when I rotated the spectacle blind? The line will be pressure tested thus, I need to rotate the spectacle to close the line. Thanks
Mar 19, 2007 1 #2 dtn6770 Mechanical Joined Jul 10, 2006 Messages 200 Location US A piping flange gasket that has had its clamping/compressive force removed should be replaced. An exception would be metal ring joint gaskets that can be reused under certain circumstances. Upvote 0 Downvote
A piping flange gasket that has had its clamping/compressive force removed should be replaced. An exception would be metal ring joint gaskets that can be reused under certain circumstances.
Mar 19, 2007 #3 pennpiper Mechanical Joined Dec 9, 2005 Messages 1,687 Location US I agree with dtn6770, You should always replace the gasket with a new one when you "break" a flanged joint. Upvote 0 Downvote
I agree with dtn6770, You should always replace the gasket with a new one when you "break" a flanged joint.
Mar 19, 2007 #4 NozzleTwister Mechanical Joined Mar 3, 2003 Messages 368 Location US Ditto, I'm also in agreement with the above replies. NozzleTwister Houston, Texas Upvote 0 Downvote
Mar 20, 2007 Thread starter #5 pipeJ123 Petroleum Joined Mar 19, 2007 Messages 2 Location NO Thanks guys! Upvote 0 Downvote