Hi all
I need help. Quick response is highly appreciated. I am currently trying to solve one problem in on production platform. during the well start up gas cap from the well is being bleed off through the flowline manifold and main line to Separator. Gas temperature in well is 6deg C and pressure is 300barg. when gas passes to the separator through the choke valve its pressure drops to 26.5barg. due to joule Thomson effect the temperature drops down to -68 deg C.
In the winter the ambient temperature is -7 deg C.
The pipe embrittlement temperature is -51 deg C.
In reality I know that gas flow will not reduce pipe wall temperature to -68 deg C because of heat transfer from air. Also I know that pipe itself has some heat.
does any body knows how I can calculate pipe inner wall temperature? I have some more questions but it will be easier for me to ask when I have answer to this question.
Thanks a lot.
I need help. Quick response is highly appreciated. I am currently trying to solve one problem in on production platform. during the well start up gas cap from the well is being bleed off through the flowline manifold and main line to Separator. Gas temperature in well is 6deg C and pressure is 300barg. when gas passes to the separator through the choke valve its pressure drops to 26.5barg. due to joule Thomson effect the temperature drops down to -68 deg C.
In the winter the ambient temperature is -7 deg C.
The pipe embrittlement temperature is -51 deg C.
In reality I know that gas flow will not reduce pipe wall temperature to -68 deg C because of heat transfer from air. Also I know that pipe itself has some heat.
does any body knows how I can calculate pipe inner wall temperature? I have some more questions but it will be easier for me to ask when I have answer to this question.
Thanks a lot.