I'm having difficulty with welding a circular base plate onto a circular column for a gantry leg.
Circular column is approx 508mmø and base plate is about 50mm thick.
Gussets welded around top of the base plate.
Due to the amount of welding on 1 side, the base plate is becoming deformed and basically starting to "dome".
I am trying to find a suitable method of stopping this happening as sometimes 2 plates have to be positioned back to back and they wont sit flat against each other.
Thanks Woody
I'm having difficulty with welding a circular base plate onto a circular column for a gantry leg.
Circular column is approx 508mmø and base plate is about 50mm thick.
Gussets welded around top of the base plate.
Due to the amount of welding on 1 side, the base plate is becoming deformed and basically starting to "dome".
I am trying to find a suitable method of stopping this happening as sometimes 2 plates have to be positioned back to back and they wont sit flat against each other.
Thanks Woody