We could use the forum's help in locating an "Expert" regarding galvanization, white rust (shipping), and it's treatment and repair at a harbor location, sea air, etc..

A Chicago area expert would be great! An recommendations regarding who to speak with would be welcomed.

rod
 
Replies continue below

Recommended for you

If we don’t have a contributor from your area post a reply these people did have knowledgeable people all over. They are quite good to work with.
If they don't have someone in your area they should be able to point you in the right direction.

 
Call Gordon Smith at H.C.Nutting/Material joining Consultants in Columbus, OH 624--863-9626. He has a wealth of experience with this issue.
 