Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

galvanic series for sulfuric acid app 2

Status
Not open for further replies.

MachinaMan

Mechanical
Joined
Aug 30, 2003
Messages
70
Location
CA
Hi All,

Is there such a thing as a galvanic series for sulfuric acid or is the acid too weak of an electrolyte to have a galvanic corrosion problem?

I have a new pump with an alloy 20 liquid end that I want to hook up to existing carbon steel (A106) piping.

Sulfuric acid concentration is 93% and is at room temperature.

Any comments?

Thanks,
 
The concentrated sulfuric acid is a strong electrolyte, hence the galvanic corrosion you have mentioned is very likely. You must prevent the electric conductivity between the pump and the C/S piping, by using suitable insulators. However, the 93% acid will not significantly corrode the C/S at 20 deg C (what is your definition of room temperature?), but over 25-28 deg C, the corrosion and erosion in C/S pipe increases considerably, hence the galvanic corrosion will be the least of your concerns.
cheers,
gr2vessels
 
MachinaMan: you didn't like the answers you were given to this question on the other thread?
 
Hi Moltenmetal,

Why would you assume that I didn't like the answers from the other thread?

As you can see, my question in this thread is considerably different than the original question.
I am trying to use this opportunity to learn about corrosion issues instead of simply asking for a recomendation for one particular application.

By the way, your previous advice was very helpful, thanks.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top