Galvanic Corrosion Potential 2

Status
Not open for further replies.

SondrupJoe

Nuclear
Jun 27, 2006
2
What are the probabilities of having "Galvanic Corrosion" occur when using galvanized ASTM A-36 material with ASTM 300 series stainless steel?
 
Replies continue below

Recommended for you

Under what conditions? It is realted to the electrical conductivity of your electrolyte. If this is atmospheric exposure you should be fine. If this will be wet it may a different situation.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 
If these two materials are coupled in the presence of an electrolyte, the probability of galvanic corrosion is 100%

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
the use is for companion angle flanges on ductwork. There are potential issues with humidity.
 