Hi Dear All,
I am working in valve industry.
Input like : Design pressure 5000 PSI, Temp. Up 10 175Deg .C. I have uplex body. material is ASTM A182-F51( UNS S31800) .i am worrying about bolting cause galling issue. what type of material should i use? i am reffering ASTM A 193, ASTM A 453,ASTM 449. but also. but i am not getting ideal from it. so can anybody help me on this matter?
I am working in valve industry.
Input like : Design pressure 5000 PSI, Temp. Up 10 175Deg .C. I have uplex body. material is ASTM A182-F51( UNS S31800) .i am worrying about bolting cause galling issue. what type of material should i use? i am reffering ASTM A 193, ASTM A 453,ASTM 449. but also. but i am not getting ideal from it. so can anybody help me on this matter?