I have an component made of aluminum, density is 0.0002538 lb sec2/in4 to keep units consistent with E in psi and size in in. I have to test this component in different crash conditions up to 12g
I checked abaqus manual,it say to insert the acceleration which is 386.09 in/sec2 (1 g) x 12 ~ 4633 in/sec2
I calculated the force the component is subject to as F=mxa = 0.0542 lb sec2/in x 4633 in/sec2 ~ 251.11 lbf
With this acceleration I barely see any stress within the component, we are talking about 500 psi! Yes the component is pretty bulky.
Am I making any mistake?
Thanks
I checked abaqus manual,it say to insert the acceleration which is 386.09 in/sec2 (1 g) x 12 ~ 4633 in/sec2
I calculated the force the component is subject to as F=mxa = 0.0542 lb sec2/in x 4633 in/sec2 ~ 251.11 lbf
With this acceleration I barely see any stress within the component, we are talking about 500 psi! Yes the component is pretty bulky.
Am I making any mistake?