Maybe we take bets on which joint? [bigsmile]
 
Mag particle or ultrasonic all the welds?

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
The many types of welding non destructive examination (Visual, PT, UT, Mag Partial, RT) are complimentary, each has it's range of flaws they find best.
It would be interesting to know what the NDE acceptance criteria of construction specification are.
If the current NDE method or acceptance criteria are different than that of construction, flaws not found previously will present, interpreting the importance of these findings importance gets messy.
 
Since the issue is likely fatigue related, then the best testing for this type of potential failure should be utilised. There should also be a schedule for future examinations established.

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Yea, I'm for x-raying the whole thing.
 
The 'Fury 325' roller-coaster is reopening:

North Carolina Roller Coaster Reopens After A Large Crack Launched A State Investigation

Carowinds amusement park staff closed Fury 325 on June 30 after a visitor reported the crack.



John R. Baker, P.E. (ret)
Irvine, CA
Siemens PLM:

The secret of life is not finding someone to live with
It's finding someone you can't live without
 
"Now at least 50% more thrilling than before!"
 