nsmith40
Mechanical
- Apr 14, 2007
- 19
I am making a splined engagement dog of about 2 inches in diameter. The stock material I have to use is 4140 pre-hardened to roughly 30 HRc.
The part will be machined then I would like the hardness to be increased to roughly 45 HRc and then finally internal splines will be cut using Wire EDM.
What processes will be required to achieve this increase in hardness?
The part will be machined then I would like the hardness to be increased to roughly 45 HRc and then finally internal splines will be cut using Wire EDM.
What processes will be required to achieve this increase in hardness?