Furnace Convection Section Remaining life analysis 1

Status
Not open for further replies.

rustbuster

Petroleum
Jul 7, 1999
289
I have been tasked with estimating remaining life of some furnace convection sections.

I am hoping some of you folks may have done similar and can offer some ideas. things that come to mind initially are;

• What types of inspection data we need
• Historical failures
• Damage mechanisms
• Structural integrity
• Refractories

I'm looking for a pro-active approach vs. reacting to failures. We have far exceed desing life.

Thanks in advance for your thoughts and experience.
 
Replies continue below

Recommended for you

If the furnace convection sections are actual tube elements, here is what I would suggest.

- review of past tube leaks, locations in the bundle and type of leaks (pin hole versus cracks versus fish mouth ruptures).
- review past operating history and try to compare actual field data (temperature and pressure) with stated operating conditions.
- inspection options will be based on known damage mechanisms, OD or ID wastage. Inspections should focus on wall thickness, ID oxide thickness, attachment welds, butt welds.
- I would schedule removal of tube samples, nothing better than getting your hands on actual furnace tube material. Send to a reputable metallurgical laboratory for general evaluation.
 
Thanks metengr,

This was the approach I proposed but I'm facing reluctance to remove sections for analysis. I have taken two shock bank samples but have little access to the upper sections (superheaters, economizers).

I was hoping someone might have justified replacements based on economics, energy savings, etc.

 