We are carrying out full penetration weld joints in one of our project. But the customer specification does not call for carrying out volumetric NDE (i.e. RT/UT) of weld joints.So we are not carrying out RT/UT of weld joints.
But QC engineer is asking if you are not carrying out volumetric NDE, how you will ensure that the joint is full penetration weld joint?
We replied that we have done the weld configuration as per drg (i.e. root face, root gap, weld edge angle). Also back chipping is done.
All this is adequate to prove that the joint is full penetration weld joint.
Experts are requested to comment on how to ensure that the joint is full penetration weld joint without carrying out volumetric NDE.
But QC engineer is asking if you are not carrying out volumetric NDE, how you will ensure that the joint is full penetration weld joint?
We replied that we have done the weld configuration as per drg (i.e. root face, root gap, weld edge angle). Also back chipping is done.
All this is adequate to prove that the joint is full penetration weld joint.
Experts are requested to comment on how to ensure that the joint is full penetration weld joint without carrying out volumetric NDE.