A client's specification regarding FRP pipe and fittings reference requirement for DSC (Differential Scanning Calorimetry)testing. First time I have encountered such testing requirement. Is this test common or some rarely used test??
Appreciate any comments and thank you for your attention regarding this matter.
 
DSC is lab test method,used mainly to found out Tg of material. It is common to use it at sampling and during re-qualification stage.
 