Dear all,
we select FRP equipment working in nitration process, and some failure occured during operation, especially for flange face and agitator part.so, does anyone have relative practical experience about this kind of equipment in nitration process?
is it necessay to update materials to replace FRP, or maybe much more focusing on FRP fabrication and operation process?
photo shows detail information in flange face.
Thank you.
we select FRP equipment working in nitration process, and some failure occured during operation, especially for flange face and agitator part.so, does anyone have relative practical experience about this kind of equipment in nitration process?
is it necessay to update materials to replace FRP, or maybe much more focusing on FRP fabrication and operation process?
photo shows detail information in flange face.
Thank you.