gbpackerman
Geotechnical
- Dec 10, 2002
- 2
We have an attached concrete garage frost wall that has developed three cracks top to bottom about one month after pouring. the cracks widened to about 1" and top of wall dropped 3/4" over the next three weeks. Hand auger borings probes performed to about 2' below footings. Static cone penetrometer testing was performed as probes were advanced. Subgrade soils consisted of natural brown to gray/brown silty clay & exhibited very stiff to hard consistency with estimated unconfined compressive strengths of 1.5 to 4.0 tsf. Free water was not encountered. Testing did not offer conclusive causality for the cracks. Any suggestions?