Hello, I'm a Civil Engr. and cannot find this info. Does anyone know what the friction factor is between two sheets of polyurethane as one a pulled across the other.

Richard A. Cornelius, P.E.
 
It depends very much on the grade of PU.

Contact the raw material manufacturer for details on their specific grade

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
There will be a lot of friction between two elastomers. However, as Pat said, PU is not one material, there are thousands of different types, each with a different coefficient of friction. In fact, all PVC flooring is coated with polyurethane to improve wear resistance and to tune the gloss and friction levels.

Chris DeArmitt

"Knowledge has no value except that which can be gained from its application toward some worthwhile end."
Think and Grow Rich - Napoleon Hill
 