Friction / Damping Calc

Status
Not open for further replies.

CondensedMatter

Mechanical
Nov 7, 2006
19
I'm designing a spring with spring washers (belleville type).

I'm looking for formulas to calculate the damping / frictional effects of stacking them unidirectionally.

The stress / deflection formulas are easily found.

 
Replies continue below

Recommended for you

Key Bellevilles list the hysteresis in parallel unlubricated stacks as

2 +/- 4 to 6%
3 +/- 6 to 9%
4 +/- 8 to 12%
5 +/- 10 to 15%

The "+" is the gain in force on compression and the "-" is the decrease in force on relaxation.
 