i recently had a basement slab poured for our new home as contractor was finishing it rained very hard for about 40 min.the slab is 2300 sq ft and has 5 " of gravel,1" polystyrene foam,radiant floor barrier,10 guage remesh, radiant heat tubing and fiber mesh added to concrete.slab is app 4.5" thick and leading edge at walkout basement wall is app 10" thick.he did not cover slab and a lot of the top layer was washed away.he then added portland cement to floor and flinshed it as best as he could.we had plans to acid stain floor and now it has power trowel marks ,several dark areas (i think this is the portland) and finish is uneven and not as smooth as concrete i have had poured in past.is this floor sound enough for our house?can it still be stained? should i have concrete tested and what test should i have done? i'm i need of professsional advice as i dont know what to do from here.thanks mbed