charnott
Civil/Environmental
- Apr 11, 2012
- 46
As Program Manager on a large scheme we are concerned by in-situ density test results which regularly show compaction >100% of sampled MDD. The Engineering Design Consultant's specification to which the Contractor is working states that Lab OMC/MDD should be tested 'once a week'. With the contractor currently producing 10,000m3/week and planned production to recah 42,000m3/week I am concerned that the specified frequency is not appropriate and am planning to raise an RFI to the designer asking for his review of this issue.
COuld there be any other reason compactions >100% are being reported?
For information: the material is sand, <15% fines, 100% passing 75mm sieve.
Thanks in advance
COuld there be any other reason compactions >100% are being reported?
For information: the material is sand, <15% fines, 100% passing 75mm sieve.
Thanks in advance