Apr 8, 2004 #1 facca Civil/Environmental Joined Mar 27, 2004 Messages 37 Location CA I have long held the position that the reliability of the salt scaling freeze test is suspect.This has been confirmed on a recent project where the highway agencies QA results past and my QC failed after just ten cycles.
I have long held the position that the reliability of the salt scaling freeze test is suspect.This has been confirmed on a recent project where the highway agencies QA results past and my QC failed after just ten cycles.