Have used Cd4Mcu on brine concentrator pump units previously, this were 24" end suction units, I read your post as looking for a manufacturer which I guess is the first step and would think that materials wouldn't be a problem with a large manufacturer. Unfortunately I have no direct experience with Francis turbine and the 2 links given were off the top of my head as likely source.