In many metals the fracture toughness increases as the strength (and hardness) increases, until you get to a tipping point where there is not enough remaining ductility to blunt crack propagation, then toughness drops with increasing strength and hardness.
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube