hi all,
I have one question for your attention on test material...
I know that for the torsion test i have:
1)Shear (ductile) failure is along the maximum shear plane (90 degreed)
2) Tensile (brittle) failure is perpendicular to the maximum
tensile stress (at 45o), resulting in a helical fracture
The question is:
only in torsion test i have this difference behavior for the surface failure between brittle and ductile material while for tensile and bendig testing i have always the surface failre perpedicular to maximum stress?
Tanks and best regards
 
Replies continue below

Recommended for you

Because you do not usually get high enough shear loads in those tests to get shear failures.
 
A cylindrically shaped ductile tensile specimen will fail in a typical cup-cone configuration along shear planes rather than transverse (perpendicular).

Maybe someone will provide a link showing a photograph of a cup-cone failure. One picture is worth a lot of words.

 
Here is a link:

Scroll down to Fig. 8.1 and 8.3

Quote from my above post:
...ductile tensile specimen will fail in a typical cup-cone configuration along shear planes rather...

I should have said,"...primarily along shear planes..."

In the above post, I was visualizing a failure between Fig. 8.1a and 8.1b where the cup is much deeper and there is very little transverse fracture face, maybe even rounded. However, Fig. 8.1a certainly belies a perpendicular fracture face. The author states this condition (8.1a) as highly ductile but maybe he meant ideally ductile (not to be expected in reality). And yet I suppose I can picture a piece of cylindrical shaped pure Lead rupturing to a point?
 